Static Crack Repair Sample Clauses
Static Crack Repair a. The Contractor shall ensure that all static cracks (not to exceed 1/32in x 1/32in) shall be cleaned out and opened to a “V” configuration.
b. The Contractor shall fill all prepared static cracks with patch or caulking material to match the existing texture as closely as possible.